Exfoliace karabiny v prost edí krasové jeskyně

DOI: 10.2478/v10227-011-0001-z

Full-Text   Cite this paper   Add to My Lib

Abstract:

The study presents an interesting example of exfoliation of aluminium alloy. The snap-link was exposed to a karst cave environment. Each part of the security set was observed by means of an optical and scanning electron microscope with EDS analyzer. Corrosion products were analyzed by X-ray diffraction (XRD). The snap-link failure was caused by an inappropriate heat treatment and exposure to a permanently humid atmosphere.