Bond strength of endodontic sealers after intracanal surface pretreatment with CO2 laser

Keywords: adhesion , sealers , Endodontics , CO2 laser.

Full-Text   Cite this paper   Add to My Lib

Abstract:

Introduction: The aim of this study was to evaluate in vitro the bonding of AH Plus and Endofill sealers to intraradicular canal walls after different dentin surface treatments. Material and methods: Sixty canines were sectioned obtaining dentin discs with 4-mm thickness and were embedded in acrylic resin. The canals were prepared with diamond burs. The specimens were divided into two groups(n = 30): GI – AH Plus and GII – Endofill and were subdivided into three groups based on the dentin surface treatment (n = 10): A – distilled and deionized water (control), B – 17% EDTA, C – CO2 laser with 3W in continuous mode for 10s. The specimens were submitted to push out test in a universal testing machine. Results: Tukey test revealed that the IB (AH Plus/17% EDTA) (17.59 ± 6.04) and IC (AH Plus/CO2 laser) (21.69 ± 4.93) subgroups had the highest values, which were statistically similar between each other (p > 0.05) and different from the other subgroups (p < 0.05). IIC subgroup (Endofill/CO2 laser)(7.25 ± 1.59) had intermediate values, which were statistically similar to (p > 0.05) IA subgroup (AH Plus/water) (10.99 ± 2.63), IIA subgroup Endofill/water) (3.16 ± 0.83) and IIB subgroup (Endofill/ 17% EDTA)(5.31 ± 3.61), which had the smallest values (p < 0.05). Conclusion: The treatment of superficial intracanal dentin with CO2 laser and EDTA favored the adhesion of AH Plus and Endofill sealers.

Full-Text

comments powered by Disqus

Contact Us

service@oalib.com

QQ:3279437679

WhatsApp +8615387084133

WeChat 1538708413