纳秒脉冲激光去除铝合金表面氧化膜数值模拟与试验研究
Numerical Simulation and Experimental Study of Nanosecond Pulsed Laser Removal of Oxide Film on Aluminum Alloy Surface

DOI: 10.12677/app.2024.146047, PP. 424-435

Keywords: 激光清洗,7075铝合金,表面形貌,工艺参数,有限元模拟
Laser Cleaning
, 7075 Aluminum Alloy, Surface Morphology, Process Parameters, Finite Element Simulation

Full-Text   Cite this paper   Add to My Lib

Abstract:

采用纳秒脉冲激光开展了7075铝合金表面5 μm厚氧化层的清洗研究。通过仿真模拟软件建立三维移动纳秒脉冲激光清洗7075铝合金表面氧化层的有限元模型,分析不同激光参数对氧化层表面的温度场分布的影响。分析了激光清洗试样表面的微观形貌,探讨了不同激光参数下的除氧化层效果以及基材表面的损伤情况。试验结果表明:当激光功率为34 W,试样表面的氧化层被完全去除,且粗糙度最低,基材表面未发生熔化;在该参数下清洗后试样表面氧元素最低,说明此参数为清洗阈值;去除量随功率增加而增加,与模拟结果相符;在激光功率为34 W的激光参数下除氧化层后,基材表面的硬度为432 HL,大于基材硬度,说明发生了激光表面硬化。
A nanosecond pulsed laser was used to carry out a study on the cleaning of a 5 μm thick oxide layer on the surface of 7075 aluminum alloy. A finite element model of the oxide layer on the surface of 7075 aluminum alloy cleaned by a three-dimensional moving nanosecond pulsed laser was established by simulation software to analyze the influence of different laser parameters on the temperature field distribution on the surface of the oxide layer. The microscopic morphology of the laser-cleaned specimen surface was analyzed, and the effect of removing the oxide layer and the damage to the substrate surface under different laser parameters were discussed. The test results show that: when the laser power is 34 W, the oxide layer on the surface of the specimen is completely removed, the roughness is the lowest, and the surface of the substrate is not melted; the oxygen element on the surface of the specimen is the lowest after the cleaning under this parameter, which indicates that this parameter is the threshold of the cleaning; the amount of the removal increases with the increase of the power, which is by the simulation results; the hardness on the surface of the substrate after removing the oxide layer under the laser parameter of the laser power is 34 W, which is 432 HL, greater than that of the substrate. 432 HL, which is greater than the hardness of the substrate, indicating that laser surface hardening has occurred.

References

[1]  熊柏青, 闫宏伟, 张永安, 等. 我国航空铝合金产业发展战略研究[J]. 中国工程科学, 2023, 25(1): 88-95.
[2]  宋友宝, 李龙, 吕金明, 等. 7xxx系铝合金焊接研究现状与展望[J]. 中国有色金属学报, 2018, 28(3): 492-501.
[3]  Wang, H., Luo, Y., Friedman, P., et al. (2012) Warm Forming Behavior of High Strength Aluminum Alloy AA7075. Transactions of Nonferrous Metals Society of China, 22, 1-7.
[4]  Zhou, J., Wang, B., Lin, J., et al. (2014) Forming Defects in Aluminum Alloy Hot Stamping of Side-Door Impact Beam. Transactions of Nonferrous Metals Society of China, 24, 3611-3620.
[5]  丛福官, 赵刚, 田妮, 等. 7xxx系超高强铝合金的强韧化研究进展及发展趋势[J]. 轻合金加工技术, 2012, 40(10): 23-33.
[6]  陈康华, 刘允中, 刘红卫. 7075和2024铝合金的固溶组织与力学性能[J]. 中国有色金属学报, 2000, 10(6): 819-822.
[7]  Zhang, F.D., Hiu, H., Subka, C., et al. (2018) Corrosion Behavior of Laser-Cleaned AA7024 Aluminum Alloy. Applied Surface Science, No. 435, 452-461.
[8]  招观荣, 雷泽勇, 邓健, 黄灿裕. 纳秒脉冲激光在Q235表面污染漆层的清洗工艺研究[J]. 机电工程技术, 2023, 52(2): 38-41.
[9]  陈一鸣, 周龙早, 闫飞, 王军, 黎硕, 王春明. 铝合金激光清洗机理与质量评估[J]. 中国激光, 2017, 44(12): 87-94.
[10]  Ma, M.L., Wang, L.M., Li, J.F., et al. (2020) Investigation of the Surface Integrity of Q345 Steel Cleaning of Oxidized Mining Parts. Coatings, 10, Article 716.
[11]  Zhu, G.D., Wang, S.R., Cheng, W., et al. (2020) Corrosion and Wear Performance of Aircraft Skin after Laser Cleaning. Optics & Laser Technology, 132, Article ID: 106475.
[12]  邱太文, 易俊兰, 程程, 等. 纳秒脉冲激光清洗2024铝合金表面油漆涂层特性研究[J]. 激光与光电子学进展, 2021, 58(5): 168-175.
[13]  王蔚, 纪向城, 刘伟军, 等. 5083铝合金阳极氧化膜激光清洗工艺研究[J]. 中国激光, 2023, 50(4): 181-196.
[14]  单腾, 王思捷, 殷凤仕, 等. 激光清洗的典型应用及对基体表面完整性影响的研究进展[J]. 材料导报, 2021, 35(11): 11164-11173.
[15]  孙承纬. 激光辐照效应[M]. 北京: 国防工业出版社, 2001: 11-16.
[16]  郑伟. 铣削镍基合金Inconel718时涂层刀具切削性能及失效机理研究[D]: [硕士学位论文]. 济南: 山东大学, 2012.

Full-Text

comments powered by Disqus

Contact Us

service@oalib.com

QQ:3279437679

WhatsApp +8615387084133