Effect of Cast Thickness and Austenitizing Temperature on Microstructure and Mechanical Properties of ADI and IADI Castings

DOI: 10.4236/ojmetal.2021.113003, PP. 21-35

Keywords: DI, ADI, IADI, Retained Austenite, Wear Resistance

Full-Text   Cite this paper   Add to My Lib

Abstract:

This investigation studies the impact strength, tensile strength, hardness, and wear behavior of thin wall austempered and intercritically austempered ductile iron samples with a chemical composition of 3.37% C, 2.7% Si, 0.30% Mn, 0.01% S, and 0.01% P. The austempered samples were austenitized at 900?C for 1 h and rapidly quenched in a salt bath furnace at 375?C for 1 h. The intercritically austempered samples were sub-austenitized at 810?C for 1 h and rapidly quenched in a salt bath furnace at 375?C for 1 h. The properties of the austempered and intercritically austempered thin wall plates of 5, 10, and 15 mm thickness were evaluated and compared to the as-cast samples. Austempering process affects greatly the tensile properties of all cast thicknesses where ultimate strength reached 1004 MPa for 5-mm thickness. Optimum impact toughness of 40 J was obtained for the austempered samples of 10- and 15-mm thicknesses. The intercritically austempered samples showed properties between the austempered and as-cast samples. Maximum wear resistance was also reported for the austempered samples due to containing retained austenite in the structure which in turn transformed into martensite that increases well the wear resistance. Maximum ultimate strength (1056) MPa and hardness (396 HV) were obtained for 5 mm ADI sample. Maximum impact toughness (43 J) was achieved for 15 mm IADI sample due to existing of pro-eutectoid ferrite in matrix. For all As-cast, ADI and IADI irons, wear resistance decreased with increasing sample thickness. Minimum wear rate (2.22 × 10?6 g/s) was reported for 5-mm ADI sample and maximum one (15.8 × 10?6 g/s) was registered for 15-mm as-cast DI sample, at a sliding speed of 2 m/s.

References

[1]  Soliman, M., Nofal, A. and Palkowski, H. (2020) Effect of Thermo-Mechanical Processing on Structure and Properties of Dual-Phase Matrix ADI with Different Si-Contents. International Journal of Metalcasting, 14, 853-860.
https://doi.org/10.1007/s40962-020-00477-4
[2]  Guesser, W.L., Lopes, C.L. and Bernardini, P.A.N. (2020) Austempered Ductile Iron with Dual Microstructures: Effect of Initial Microstructure on the Austenitizing Process. International Journal of Metalcasting, 14, 717-727.
https://doi.org/10.1007/s40962-019-00397-y
[3]  Uyar, A., Sahin, O., Nalcaci, B. and Kilicli, V. (2021) Effect of Austempering Times on the Microstructures and Mechanical Properties of Dual-Matrix Structure Austempered Ductile Iron (DMS-ADI). International Journal of Metalcasting.
https://doi.org/10.1007/s40962-021-00617-4
[4]  Janowak, J.F. and Norton, P.A. (1985) A Guide to Mechanical Properties Possible by Austempering, 1 Spercent Ni, 0.3 Percent Mo Iron. AFS Transactions, 88, 123-135.
[5]  Janowak, J.F., Gundlach, R.B., Eldis, G.T. and Rohrting, K. (1982) Technical Advances in Cast Iron Metallurgy. International Cast Metal Journal, 6, 28-42.
[6]  Kobayashi, T. and Yamada, S. (1996) Effect of Holding Time in the (α + γ) Temperature Range on Toughness of Specially Austempered Ductile Iron. Metallurgical and Materials Transactions A, 27, 1961-1971.
https://doi.org/10.1007/BF02651945
[7]  Cerah, M., Kocatepe, K. and Erdogan, M. (2005) Influence of Martensite Volume Fraction and Tempering Time on Tensile Properties of Partially Austenitized in the (α + γ) Temperature Range and Quenched + Tempered Ferritic Ductile Iron. Journal of Materials Science, 40, 3453-3459.
https://doi.org/10.1007/s10853-005-0415-3
[8]  Machado, H.D., Aristizabal-Sierra, R., Garcia-Mateo, C. and Toda-Caraballo, I. (2020) Effect of the Starting Microstructure in the Formation of Austenite at the Intercritical Range in Ductile Iron Alloyed with Nickel and Copper. International Journal of Metalcasting, 14, 836-845.
https://doi.org/10.1007/s40962-020-00450-1
[9]  Galarreta, I.A., Boeri, R.E. and Sikora, J.A. (1997) Free Ferrite in Pearlitic Ductile Iron—Morphology and Its Influence on Mechanical Properties. International Journal of Cast Metals Research, 9, 353-358.
https://doi.org/10.1080/13640461.1997.11819677
[10]  Kowalski, A., Kluska-Nawarecka, S. and Regulski, K. (2013) ADI after Austenitising from Intercritical Temperature. Archives of Foundry Engineering, 13, 81-88.
https://doi.org/10.2478/afe-2013-0016
[11]  Hayes, W.J., Martrone, H.A. and Johnson, P.D. (1989) Process of Making an Austempered Ductle Ron Article. U.S. Patent No. 4880477A.
[12]  Panneerselvam, S., Martis, C.J., Putatunda, S.K. and Boileau, J.M. (2015) An Investigation on the Stability of Austenite in Austempered Ductile Cast Iron (ADI). Materials Science and Engineering: A, 626, 237-246.
https://doi.org/10.1016/j.msea.2014.12.038
[13]  Vechet, S., Kohout, J. and Klakurkova, L. (2008) Fatigue Properties of Austempered Ductile Iron in Dependence on Transformation Temperature. Materials Science, 14, 324-327.
[14]  Ovali, I., Kilicli, V. and Erdogan, M. (2013) Effect of Microstructure on Fatigue Strength of Intercritically Austenitized and Austempered Ductile Irons with Dual Matrix Structures. ISIJ International, 53, 375-381.
https://doi.org/10.2355/isijinternational.53.375
[15]  Sellamuthu, P., Samuel, D.G. H., Dinakaran, D., Premkumar, V.P., Li, Z. and Seetharaman, S. (2018) Austempered Ductile Iron (ADI): Influence of Austempering Temperature on Microstructure, Mechanical and Wear Properties and Energy Consumption. Metals, 8, Article No. 53.
https://doi.org/10.3390/met8010053
[16]  Putatunda, S.K., Panneerselvam, S. and Alshwigi, M. (2015) Development of Nanostructured Austempered Ductile Cast Iron (ADI). 28th Heat Treating Society Conference, Detroit, 20-22 October 2015, 71-75.
[17]  Cardoso, P.H. S., Israel, C.L. and Strohaecker, T.R. (2014) Abrasive Wear in Austempered Ductile Irons: A Comparison with White Cast Irons. Wear, 313, 29-33.
https://doi.org/10.1016/j.wear.2014.02.009
[18]  Rocha-Reséndez, R. and Calderon, F.A. (2018) Corrosion Behavior of Austempered Ductile Iron Used in the Aeronautical Industry Evaluated on Acid Solutions. International Materials Research Congress 2016, Cancún, 14-19 August 2016, 73-82.
https://doi.org/10.1007/978-3-319-65611-3_7
[19]  Aristizabal, R., Foley, R., Griffin, J. and Monroe, C. (2014) Austemperability of Intercritically Austempered Ductile Iron (IADI). AFS Transactions, 279-286.
[20]  Gundlach, R. and Boileau, J. (2017) Influence of Intercritical Austempering on the Microstructure and Mechanical Properties of Ausempered Ductile Iron (ADI). Materials Science and Engineering: A, 694, 72-80.
https://doi.org/10.1016/j.msea.2017.03.096
[21]  Górny, M. and Tyrała, E. (2013) Effect of Cooling Rate on Microstructure and Mechanical Properties of Thin-Walled Ductile Iron Castings. Journal of Materials Engineering and Performance, 22, 300-305.
https://doi.org/10.1007/s11665-012-0233-0
[22]  Vélez, J.M., Tanaka, D.K., Sinatora, A. and Tschiptschin, A.P. (2001) Evaluation of Abrasive Wear of Ductile Cast Iron in a Single Pass Pendulum Device. Wear, 251, 1315-1319.
https://doi.org/10.1016/S0043-1648(01)00760-8

Full-Text

Contact Us

service@oalib.com

QQ:3279437679

WhatsApp +8615387084133